Magic-Glos 5-Inclusion UV Resin Faux Opal by Karen A. Scofield

Trial Runs: Transparent Resin Faux Opal Goddess Pendant Using Magic-Glos UV Resin

 And a much better result with a newfound inclusion.

Instagram screen capture of Goddess Pendant resn faux opal shown in different lighting. Karen A. Scofield.

Instagram screen capture of Goddess Pendant resn faux opal shown in different lighting. Karen A. Scofield.

 

Why Trial Runs Using Magic-Glos Resin?

Lisa Pavelka’s Magic-Glos UV Resin allows me to work fast (layers cure in 15 minutes), build a focal bead in layers, and experiment. I’m using this resin to try out some new products, techniques, combinations, and sequences as I learn my preferences in resin faux opal making.

Sure, it’s more expensive per ounce, but ruining a whole batch or three of a dozen or more beads at a time is even more disheartening. If I didn’t allow for a leaning curve like this first, I probably would have given up on resin. It can take months or years to really master the medium. (Things are ridiculously easy in our mind’s eye if our imagination isn’t informed by experience and tried and trusted knowledge base.)

So, here are some of my best results so far, note the slight amber tone at this depth with this resin, and I’m about to Faux Opals in Ice Resin and ArtResin. (See How to Ice Resin, How to ArtResin.) At this thickness, I expect almost no amber tone with Ice Resin and no detectable amber tone with ArtResin.

Magic-Glos Resin Tips

1. Don’t seal paper or cardstock inclusions with Mod Podge or PVC (white craft) glues if you’re using them with Magic-Glos — reactions between water-activated mediums, inks, and Magic-Glos can occur over time.

2. Bubbles can be prevented almost all the time. Read resouces given here. Bubbles can be removed by letting cured item sit one hour, drilling a hole into the bubble, cleaning up drilling debris, adding just enough Magic-Glos, and curing again.

Things Magic-Glos Doesn’t Work Well With

  • PVC glues – your white craft, nearly all decoupage mediums/glues, and school glues are PVC glues — https://thebluebottletree.com/what-is-the-difference-between-mod-podge-and-acrylic-medium
  • Air–dry glues — air-dry glues get trapped under things, don’t cure 100%, then release air bubbles into your curing resin. Use two-part epoxy glue instead!
  • Ice Resin, whether or not each resin is cured or wet (insured) — chemical reaction between the two resins causes cloudiness
  • Water-based sealants – any sealants that are not waterproof after drying (water resistant is not waterproof)
  • Alcohol inks
  • Unsealed inkjet prints
  • Anything that may run or bleed if wet
  • Sharpie markers

If in doubt, test first, often weeks ahead to make doubly sure.

Baking Magic-Glos

Don’t. Don’t bake Magic-Glos. Avoid temperatures over 100 degrees F. See MSDS.

Warning: Baking Magic-Glos with polymer clay will cause the resin to amber (brown). See MSDS sheet (link given above) for further info.

Magic-Glos Layers

Doming, Pulling Away, and Self-Leveling Properties and What They Mean to the User — The same properties that allow Magic-Glos to dome causes the resin to pull away from edges/periphery in first layer or two, hence a good dome is built up in layers, each of which are cured before the next is added. The last layers are minimal amounts and it may help to spread the resin nearly to the edge (with a toothpick or small ballpoint stylus) and then let Magic-Glos self-leveling finish the job, finally fully covering evenly and doming. Let it sit 10 minutes to 1/2 hour out of UV light to let it finish self-leveling and to let air bubbles make themselves evident. The self-leveling properties mean that you might think you only added enough, the self-doming is a bit of a delayed reaction, and then suddenly you have Magic-Glos running over the sides. If still uncured, it can be cleaned up with cotton swabs and wet wipes but prevention is better than damage control. Prevention involves adding thinner, multiple layers that are each cured before the next is added and curing your item while on a pedestal — a bit of polymer clay or poster-tx on a craft mirror a bit larger than your piece but small enough to fit in the UV lamp oven.

If the overfill cured, it can be pried off with your hands and/or chipped off with a craft knife.

Minimum Number Of Layers — usually 2 layers, less is more, meaning it’s better to add thin/incomplete layers than to overfill. Thinner layers allows the air bubble popping method of passing a butane mini torch or windproof lighter over the surface of the Magic-Glos for one and only one second.

My Latest Faux Opal Using lMagic-Glos UV Resin, by Karen A. Scofield. March 2, 2017.

My Latest Resin Faux Opal

Resin Faux Opal by Karen A. Scofield. March 2, 2017. Magic-Glos, a UV-curing redin, and various inclusions were used and the gem was built up in layers.

Materials Used (Not a Complete List):

  • Lisa Pavelka Magic-Glos Resin
  • Lisa Pavelka UV Lamp Oven thingie
  • Various Glitters
My Latest Faux Opal Using lMagic-Glos UV Resin, by Karen A. Scofield. March 2, 2017.

My Latest Faux Opal Using lMagic-Glos UV Resin, by Karen A. Scofield. March 2, 2017.

Viva Decor Precious Metal Colour Paint in Gold Was Heat-set on Cured Premo Polymer Clay, by Karen A. Scofield

Viva Decor Precious Metal Colour Heat-Set on Premo Polymer Clay

The Clay

I added crushed, shiny micaceous (meaning it’s loaded with mica) rock, fine gold glitter, and Blank Slate Gold and Silver Flake Mix, in order of volume, to some Premo! polymer clay (a Sculpey product). That’s why it’s sparkly and can appear darker or very light depending on how the light shines on it and it moves, you see sparkles as well as flashes and glints.

Aside: The Backstory on the Micaceous Rockhttps://www.flickr.com/photos/sari0009/19354330223/in/dateposted-..

The Paint (and A Closed US Office)

Spelling

Viva Decor’s US office closed in 2015 and my bottle is labeled “Precious Metal Colour” because that is how the UK spells it. Many sites and blogs still use the US spelling (Precious Metal Color), you may notice.

Viva Decor Closed Their USA Office in 2015. European Offices remain open. 2016.

Viva Decor Closed Their USA Office in 2015. European Offices remain open. 2016.

Inclusions Added to the Paint

Precious Metal Colour gold colored paint, specifically, has larger glitter-like particles while the mica powder has super fine (!) particles.

  • Alone, Pearl-Ex mica powder has a very slight orangish undertone by comparison.
  • Alone, Previous Metal Color is a bit bright and silvery.
  • Combined, the color is amazing and the larger particles of the paint aren’t glaringly evident.

So, I added a decent amount of Pearl Ex mica powder to Viva Decor “Precious Metal Colour.”

Rule: With mica powder, less is more, meaning you start by adding very small amounts and adjust according to your liking. I found my mix pleasing as a 14 karat gold color.

This doctored up Viva Decor “Precious Metal Colour” acrylic/enamel paint was painted in 3 or 4 layers on an already baked Premo polymer clay mix.

The bezels were entirely painted with the paint while the figurative beads only had detail work painted.

Heat-setting

All but one were heat-set at 275°F  for 30 minutes. There was no visual or tactile difference between the baked and unbaked paint.

I couldn’t scratch the paint off with a fingernail once the paint was heat-set. The paint looks the most like real gold. I finally, after years of looking for a rather durable solution, now have a tremendous amount of confidence regarding gold detail work on my beads and pendants.

Although Varathane Gloss sealant is one of the top choices for sealing polymer clay, it’s water-resistant, not waterproof. I’d prefer not to have to seal my beads at all.

Acrylic Paints — Drying Time vs. Cured

Note: There is A difference between drying time in curing time. Drying time might occur within minutes or a few hours for acrylic paints while curing time might take a few days. This difference might help explain some problems with heat-setting acrylic paints a polymer clay.

I say it might help explain some of the problems because, according to Blue Bottle Tree, there was a correlation between painting the paint on raw polymer clay before heat-setting and the paint bubbling. This was dependent upon brand of acrylic paint and/or polymer clay, whether the clay was raw or cured, and other factors. For more information, see that Blue Bottle Tree blog post.

One Minor Problem to Solve

When removing these painted bezels from the glossy tile they were baked on, some of the gold paint stuck to the tile. There was enough paint remaining on the bezels so this wasn’t a problem but I’d would still prefer this not  happen.

Perhaps baking on a silicone mat would improve things.

Magic-Glos with Tiny Clay Sculpture and Inclusions by Karen A. Scofield.

Jewelry Resin (Magic-Glos, Ice Resin) Tiny Sculptures, and Bezels

Magic-Glos

Spelling –Magic-Glos is hyphenated and is spelled with only one “s.”

I’m going to discuss Magic-Glos here more because Ice Resin has books based on it. One such book is “Resin Alchemy: Innovative Techniques for Mixed-Media and Jewelry Artists,” by Susan Lenart Kazmer.

 image

Magic-Glos Resources

Lis Pavelka’s Magic-Glos Tips: http://www.lisapavelka.com/wp-content/uploads/2015/04/Magic-Glos-Tips-Tricks-15.pdf

Magic-Glos MSDS (Material Safety Data Sheet): http://www.artclayworld.com/v/vspfiles/assets/MSDS/magic_glos.pdf

Fire Mountain Gems Magic-Glos Tips and Information: http://www.firemountaingems.com/resources/jewelry-making-articles/f35h

Corrections to My Magic-Glos Video (Always Learning!)

1. Don’t seal paper or cardstock inclusions with Mod Podge or PVC (white craft) glues if you’re using them with Magic-Glos — reactions between water-activated mediums, inks, and Magic-Glos can occur over time.

2. Bubbles can be  prevented almost all the time. Read resouces given here. Bubbles can be removed by letting cured item sit one hour, drilling a hole into the bubble, cleaning up drilling debris, adding just enough Magic-Glos, and curing again.

Things Magic-Glos Doesn’t Work Well With:

  • PVC glues – your white craft, nearly all decoupage mediums/glues, and school glues are PVC glues — https://thebluebottletree.com/what-is-the-difference-between-mod-podge-and-acrylic-medium
  • Airdry glues — air-dry glues get trapped under things, don’t cure 100%, then release air bubbles into your curing resin. Use two-part epoxy glue instead!
  • Ice Resin, whether or not each resin is cured or wet (insured) — chemical reaction between the two resins causes cloudiness
  • Water-based sealants – any sealants that are not waterproof after drying (water resistant is not waterproof)
  • Alcohol inks
  • Unsealed inkjet prints
  • Anything that may run or bleed if wet
  • Sharpie markers

If in doubt, test first, often weeks ahead to make doubly sure.

Baking Magic-Glos

Don’t. Don’t bake Magic-Glos. Avoid temperatures over 100 degrees F. See MSDS. 

Warning: Baking Magic-Glos with polymer clay will cause the resin to amber (brown). See MSDS sheet (link given above) for further info.

Magic-Glos Layers

Doming, Pulling Away, and Self-Leveling Properties and What They Mean to the User — The same properties that allow Magic-Glos to dome causes the resin to pull away from edges/periphery in first layer or two, hence a good dome is built up in layers, each of which are cured before the next is added. The last layers are minimal amounts and it may help to spread the resin nearly to the edge (with a toothpick or small ballpoint stylus) and then let Magic-Glos self-leveling finish the job, finally fully covering evenly and doming. Let it sit 10 minutes to 1/2 hour out of UV light to let it finish self-leveling and to let air bubbles make themselves evident. The self-leveling properties mean that you might think you only added enough, the self-doming is a bit of a delayed reaction, and then suddenly you have Magic-Glos running over the sides. If still uncured, it can be cleaned up with cotton swabs and wet wipes but prevention is better than damage control.  Prevention involves adding thinner, multiple layers that are each cured before the next is added and curing your item while on a pedestal — a bit of polymer clay or poster-tx on a craft mirror a bit larger than your piece but small enough to fit in the UV lamp oven.

If the overfill cured, it can be pried off with your hands and/or chipped off with a craft knife.

Minimum Number Of Layers — usually 2 layers, less is more, meaning it’s better to add thin/incomplete layers than to overfill. Thinner layers allows the air bubble popping method of passing a butane mini torch or windproof lighter over the surface of the Magic-Glos for one and only one second.

Note: You don’t have to use seven layers like I did. I used so many layers because I made mistakes and was fiddling with different effects. You can use three layers or more, and maybe less. It depends on what you doing, of course.

Ice Resin

Ice Resin Faux Opal, by Karen A. Scofield. 2016.

Ice Resin Faux Opal, by Karen A. Scofield. 2016.

I also did a faux opal with Ice Resin. Fun!

Raised Scratch Foam Designs in Polymer Clay

Raised Scratch Foam Polymer Clay Designs

Raised Scratch Foam Designs in Polymer Clay

Raised Scratch Foam Polymer Clay Design Test, with notes, by Karen A. Scofield

KarenAScofield Spriograph Clay Texture SheetsNote: This page will be updated as examples are made.

The above picture is only a simple and fast test. It’s not meant to be a prime example, just an example to get your creative juices flowing (and mine). It shows a moon shaped piece of clay with a raised scratch foam design that was colored with Pearl Ex.

I haven’t yet seen others doing it, but yes indeedy, spirographs can be used on scratch foam (Inovart Presto Foam Printing Plate was used in this case) with a ball point pen, ball stylus, or Sakura Gel Pen.

Back at it, Dec. 2016.

KarenAScofield Spriograph Clay Texture Sheets

spirograph clay texture sheet by Karen a Scofield

The Basic Idea

Create a design on scratch foam with a spirograph set and a ball point pen. Press  polymer clay into the design and lift. Add bead holes, etc. You’re looking for spirograph sets that won’t make unintended scratches on the scratch foam. Mine came with “The Spiral Draw” Book.

Taking it Further

Pointillism elements or entire designs be be added inside or around the spirograph design with a ball point pen or ball stylus. The result creates raised clay designs once clay is preseed into it.

Ball point styluses that come in varying sizes can be used for added interest and then needles or beed hole makers can be dragged across the surface, at a slant, to add on to the design too.

Scratch foam designs are probably more commonly used for printing monoprints and other techniques … and also by metal clay artists. They can be earthy/rustic looking or linear and crisp ones.

One can create a bezel complete with boarder designs, with scratch foam designs. What you indent on the foam will be raised on the clay. If you add dimensional writer designs to the scratch foam ones, the clay pressed into it will have both raised and indented designs.

If you use Sakura Gel Pens for the spirograph scratch foam deisgns, many of their inks are oqaque and therefore show up on darker clays. You can press the clay into the fresh scratch foam design and then bake. You may want to seal your design afterward.

Any manner of polymer clay extrusions, applique, relief sculpture, lace impressions/molds, designs for faux enamels, crackling, or designs made with cutters/blades can be applied over the spirograph textured clay passages. If you’re worried about pressing clay together to cause adhesion, because you don’t want to ruin more delicate designs, you may want to use liquid clay or Bake and Bond for adhesion purposes.

With single layer or multi layered scratch foam designs, you create mixed media mosaic tiles, embellishments, beads, and larger clay sheets. You can create molds of the larger clay sheets if you want.

Raised designs can be colored with paint, Sakura Gel Pen ink, inks, or Pearl Ex powders (which are a brand of mica powder). I’d apply paint to baked clay but Sakura Gel Pen, Pearl Ex, and alcohol inks can be applied to raw clay that’s then baked.

You may want to seal baked polymer clay items that have Pearl Ex mica powders or Gel Pens baked onto them. Varathane Water Based varnish is a wonderful sealant for polymer clay pieces.